Restoring Damaged and Corroded Polished Surfaces

Reviewed by Tom Harrison, member of the ASME BPE Surface Finish Subcommittee · Updated November 2026
The short answer: Impact, abrasion, erosion, corrosion and rouge all degrade a polished surface, and in most cases the surface can be restored rather than the equipment replaced. Harrison combines pickling, mechanical polishing and electropolishing to repair damage and return the surface to its specified finish, then passivates and verifies it. Work is done in the Houston facility or on-site in the Houston area and along the Gulf Coast.
How a surface is restored
Scratches, gouges and pitting are removed by mechanical polishing to below the depth of the damage. Scale, heat tint and heavy corrosion are removed by pickling. Rouge is removed chemically or by polishing depending on type. The surface is then electropolished to recover the specified Ra and a passive, chromium-rich finish, and passivation is verified by copper-sulfate or ferroxyl testing. Ra is measured and reported where a finish was specified.
What can be restored
Vessels, reactors and tanks; process piping and manifolds; valves, pumps and fittings; agitators and mixers; conveyor screws and belts; heat exchangers; and bioprocess equipment that has rouged in service. Equipment that cannot be shipped is treated in place. See Rouge Removal & De-Rouging and Pickling and Passivation.
When restoration is not the answer
Cracks, through-wall pitting and damage deeper than the allowable wall loss are repair or replacement items, not finishing items. Harrison will say so after inspection rather than polish over a problem.
Damaged or corroded surface on equipment you'd rather restore than replace? Send photos and dimensions and we'll tell you what's recoverable and whether it can be done on-site.
Send Us Your Drawing or call 800-245-5707, Mon–Fri 7–5 Central.
Related: Mechanical Polishing · Electropolishing · Houston & Gulf Coast Service
Frequently asked questions
Can a scratched electropolished surface be repaired?
Yes. The scratch is removed by mechanical polishing to below its depth, and the area is re-electropolished to blend the finish and restore the passive surface.
Can you restore equipment without removing it from service?
Passivation, pickling and de-rouging can be performed on installed equipment in the Houston area and along the Gulf Coast. Electropolishing is performed in the Houston shop.
How do you verify the restored surface?
Passivation is verified by copper-sulfate or ferroxyl testing per ASTM A967, and surface roughness is measured with a profilometer and reported where a finish is specified.

Services
Resources
13002 Brittmoore Park Dr
Houston, TX 77041-7231
Phone: 800-245-5707