The short answer: All stainless steel corrosion starts on or near the surface, at free iron, sulfide inclusions, embedded abrasive and smeared metal left by fabrication and handling. Electropolishing dissolves that contaminated layer and leaves a surface with a higher chromium-to-iron ratio and a thicker, more uniform chromium-oxide passive film. Passivation per ASTM A967 removes the free iron without removing metal. Both measurably improve corrosion resistance; electropolishing improves it most.
Where corrosion comes from
Cutting, forming, welding, machining and polishing all contaminate the surface. Tool steel transfers iron, abrasives embed in the surface, welding leaves chromium-depleted heat tint, and handling adds grease and dirt. Each contaminant disrupts the passive film and becomes a site for pitting, crevice corrosion or rouge. Stainless steel is only as corrosion-resistant as its surface condition.
What electropolishing changes
Electropolishing removes 0.0003" to 0.0007" from the surface, taking the contaminated layer with it. Iron dissolves preferentially, so the surface becomes chromium-enriched, and the smoother profile has less area and fewer crevices for chlorides to concentrate in. Electropolishing per ASTM B912 is a recognized passivation method in its own right. See What Is Electropolishing?.
What passivation changes
Passivation in nitric or citric acid removes free iron and lets the passive film re-form, without changing dimensions or finish. It is the right choice after machining or maintenance when the finish is already acceptable, and after pickling on welded fabrications. Harrison verifies passivation with copper-sulfate and ferroxyl tests. See Stainless Steel Passivation and Electropolishing vs. Passivation.
Materials and standards
Harrison electropolishes and passivates 304, 316 and 316L stainless, AL6XN, Hastelloy and nickel alloys, and passivates titanium, to ASTM A967, ASTM A380, ASTM B912 and SAE AMS 2700 (which replaced QQ-P-35). See Materials.
Pitting, rust spots or rouge showing up on stainless equipment? Send photos and the alloy and we'll recommend passivation, electropolishing or pickling plus passivation.
Send Us Your Drawing or call 800-245-5707, Mon–Fri 7–5 Central.
Related: Passivation Services · Stainless Steel Electropolishing · Rouge Removal
Frequently asked questions
Why does stainless steel rust?
Stainless steel resists corrosion through a thin chromium-oxide passive film. Free iron, embedded abrasive, inclusions and heat tint left by fabrication break that film locally, and corrosion starts at those points. Removing the contaminants restores the resistance.
Which improves corrosion resistance more, electropolishing or passivation?
Electropolishing. It removes the contaminated surface layer and leaves a chromium-enriched, smoother surface. Passivation removes free iron only, which is sufficient when the finish is acceptable and the surface is not heavily worked.
What standard should I specify?
ASTM A967 for chemical passivation, ASTM B912 for passivation by electropolishing, and SAE AMS 2700 for aerospace work. Name the standard and the verification test on the purchase order.